A 'thermoplastic' is a material that is
plastic or deformable,
melts to a liquid when heated and freezes to a
brittle,
glassy state when cooled sufficiently. Most thermoplastics are high
molecular weight polymers whose
chains associate through weak
van der Waals forces (
polyethylene); stronger
dipole-dipole interactions and
hydrogen bonding (
nylon); or even stacking of
aromatic rings (
polystyrene). Thermoplastic polymers differ from
thermosetting polymers (
Bakelite;
vulcanized rubber) as they can, unlike thermosetting polymers, be remelted and remoulded. Many thermoplastic materials are
addition polymers; e.g.,
vinyl chain-growth polymers such as polyethylene and
polypropylene.
Temperature dependence

Stress strain graph of thermoplastic material
Thermoplastics are elastic and flexible above a
glass transition temperature ''T''
g, specific for each one — the midpoint of a
temperature range in contrast to the sharp
freezing point of a pure
crystalline substance like
water. Below a second, higher melting temperature, ''T''
m, also the midpoint of a range, most thermoplastics have crystalline regions alternating with
amorphous regions in which the chains approximate
random coils. The amorphous regions contribute
elasticity and the crystalline regions contribute strength and rigidity, as is also the case for non-thermoplastic
fibrous proteins such as
silk. (Elasticity does not mean they are particularly stretchy; e.g., nylon
rope and
fishing line.) Above ''T''
m all crystalline structure disappears and the chains become randomly inter dispersed. As the temperature increases above ''T''
m,
viscosity gradually decreases without any distinct
phase change.
Thermoplastics can go through melting/freezing cycles repeatedly and the fact that they can be reshaped upon reheating gives them their name. This quality makes thermoplastics recyclable. The processes required for recycling vary with the thermoplast. The plastics used for pop bottles are a common example of thermoplastics that can be and are widely recycled.
Animal horn, made of the
protein α-keratin, softens on heating, is somewhat reshapable, and may be regarded as a natural, quasi-thermoplastic material.
Some thermoplastics normally do not crystallize: they are termed "amorphous" plastics and are useful at temperatures below the ''T''
g. They are frequently used in applications where clarity is important. Some typical examples of amorphous thermoplastics are PMMA, PS and PC. Generally, amorphous thermoplastics are less chemically resistant and can be subject to
stress cracking. thermoplastics will crystallize to a certain extent and are called "semi-crystalline" for this reason. Typical semi-crystalline thermoplastics are PE, PP, PBT and PET. The speed and extent to which crystallization can occur depends in part on the flexibility of the polymer chain. Semi-crystalline thermoplastics are more resistant to solvents and other chemicals. If the crystallites are larger than the wavelength of light, the thermoplastic is hazy or opaque.
Semi-crystalline thermoplastics become less brittle above ''T''
g. If a plastic with otherwise desirable properties has too high a ''T''
g, it can often be lowered by adding a low-molecular-weight
plasticizer to the melt before forming (
Plastics extrusion;
molding) and cooling. A similar result can sometimes be achieved by adding non-reactive
side chains to the
monomers before
polymerization. Both methods make the polymer chains stand off a bit from one another. Before the introduction of plasticizers,
plastic automobile parts often cracked in cold
winter weather. Another method of lowering ''T''
g (or raising ''T''
m) is to incorporate the original plastic into a
copolymer, as with
graft copolymers of polystyrene, or into a
composite material. Lowering ''T''
g is not the only way to reduce brittleness.
Drawing (and similar processes that stretch or orient the molecules) or increasing the length of the polymer chains also decrease brittleness.
Although modestly vulcanized natural and synthetic rubbers are stretchy, they are
elastomeric thermosets, not thermoplastics. Each has its own ''T''
g, and will crack and shatter when cold enough so that the
crosslinked polymer chains can no longer move relative to one another. But they have no ''T''
m and will decompose at high temperatures rather than melt. Recently,
thermoplastic elastomers have become available.
List of thermoplastics
★
Acrylonitrile butadiene styrene (ABS)
★
Acrylic
★
Celluloid
★
Cellulose acetate
★
Ethylene-Vinyl Acetate (EVA)
★
Ethylene vinyl alcohol (EVAL)
★
Fluoroplastics (PTFEs, including FEP, PFA, CTFE, ECTFE, ETFE)
★
Ionomers
★
Kydex, a trademarked acrylic/PVC
alloy
★
Liquid Crystal Polymer (LCP)
★
Polyacetal (POM or Acetal)
★
Polyacrylates (Acrylic)
★
Polyacrylonitrile (PAN or Acrylonitrile)
★
Polyamide (PA or Nylon)
★
Polyamide-imide (PAI)
★
Polyaryletherketone (PAEK or Ketone)
★
Polybutadiene (PBD)
★
Polybutylene (PB)
★
Polybutylene terephthalate (PBT)
★
Polyethylene terephthalate (PET)
★
Polycyclohexylene dimethylene terephthalate (PCT)
★
Polycarbonate (PC)
★
Polyhydroxyalkanoates (PHAs)
★
Polyketone (PK)
★
Polyester
★
Polyethylene (PE)
★
Polyetheretherketone (PEEK)
★
Polyetherimide (PEI)
★
Polyethersulfone (PES)- see
Polysulfone
★
Polyethylenechlorinates (PEC)
★
Polyimide (PI)
★
Polylactic acid (PLA)
★
Polymethylpentene (PMP)
★
Polyphenylene oxide (PPO)
★
Polyphenylene sulfide (PPS)
★
Polyphthalamide (PPA)
★
Polypropylene (PP)
★
Polystyrene (PS)
★
Polysulfone (PSU)
★
Polyvinyl chloride (PVC)
★
Polyvinylidene chloride (PVDC)
★
Spectralon
See also
★
Thermosetting plastic
★
Thermoplastic Elastomers for Fluid Resistance Applications